av免费片-国产精品嫩草影院8Vv8-色999-一二三四在线播放免费观看中文版视频|www.nanobeauty.net

中文 | English

上海總部:021-63040008

上海業(yè)務(wù)部:021-64618320

南京分部:025-83357941

杭州分部:0571-81990171

天津分部:022-26756760

昆明分部:0871-67163117

南寧分部:0771-3852969

廣州分部:020-36284098

福州分部:0591-88072895

武漢分部:027-88107720

成都分部:028-87623656

西安分部:029-62603771

寧波分部:0574-87225251

長春分部:0431-84480802

長沙分部:0731-89781357

合肥分部:0551-62762035

南昌分部:0791-88201213

產(chǎn)品名稱: Injection Packer-15cm

Injection Packer

 

Long packer over 15cm is for loose structure;
Short packer 8.5cm, 10cm for dense structures.
Other specifications can be customized.

 

 

Construction of high-pressure Injection Waterproofing System

 

Construction Prepares

a. Find crack: For wet surface, first clean water; for dry surface, clean dust. Carefully looking for cracks, using colored pens or chalk mark along the cracks;

b. Drilling: According to the thickness of concrete structures, from the crack of about 150 ~ 350mm, cross-drilled on both sides along the crack direction. 14mm diameter drill bit used. Holes and cracks in cross-section should be 45 degrees to 70 degrees cross, and the central cross in the bottom 1 / 2 range.

c. Bury injection packers: buried with tools and fastening to ensure that the rubber part of the needle and the hole wall are dry before use, otherwise easily lead to slip when tightening.

 

 

 

 

Construction Notes

a. First, analysis cracks’ width and length,take cores to determine the development of crack depth.

b. If the surface is not easy dry, you can use torch drying, cracks due to moisture, can be found immediately to improve efficiency.

 

 

Crack Repair

 a. Injection should be started in elevation from bottom to top, when the foam materil emerge from the cracks should immediately stop,and start again after a while. In the infusion process, if the material adjacent to the needle position has been filled, you can jump without injection. If found cracks extension in both ends or cracks with cross, should drill holes again, re-grouting .

b. To fill cracks with polyurethane, should grout again before the material become solid.

 

Notes when Grouting

a. Stop infusing if polyurethane does not emitting from the cracks after 5 minutes. And try again later. If not yet filled, should check whether the buried pipeline cross-drilled or floor have holes and so on.

b. Infusion should be closely watched gauge of work perfusion machine, if more than the rated pressure (45Mpa above), should be shut down, if pressure remained high, cracks should check whether the drilling cross with cracks.

 

Detection of Crack Repair

After complete of the cracks repair, testing with the core drilling. Test results should be the concrete surface smooth and dense, materials filled all the cracks in structure, and the compressive strength of concrete core samples meet the original design value.